SALD

Spatial Atomic Layer Deposition (SALD) is a new process that is faster and less expensive than ALD, which opens new fiels of industrial applications for flexible and large substrates (OLEDs, flat displays, photovoltaic cells…). In Spatial ALD the classical sequence of precursor injection + purge is replaced by an alternative …